1.1 This test method covers the determination of the resistance to fracture of metallic materials under Mode I loading at static rates using either of the following notched and precracked specimens: the middle-cracked tension M(T) specimen or the compact tension C(T) specimen. A KR curve is a continuous record of toughness development (resistance to crack extension) in terms of KR plotted against crack extension in the specimen as a crack is driven under an increasing stress intensity factor, K. (1)2 1.2 Materials that can be tested for KR curve development are not limited by strength, thickness, or toughness, so long as specimens are of sufficient size to remain predominantly elastic to the effective crack extension value of interest. 1.3 Specimens of standard proportions are required, but size is variable, to be adjusted for yield strength and toughness of the materials. 1.4 Only two of the many possible specimen types that could be used to develop KR
Prenumerera på standarder med tjänst SIS Abonnemang. Genom att prenumerera får du effektiv åtkomst till gällande standarder och säkerställer att ditt företag alltid har tillgång till senaste utgåvan.
Läs mer om SIS Abonnemang